NASA's 3D-printed superalloy can take the heat
GRX-810 is an oxide dispersion strengthened alloy. In other words, tiny particles containing oxygen atoms spread throughout the alloy enhance its strength. Such alloys are excellent candidates to build aerospace parts for high-temperature applications, like those inside aircraft and rocket engines, because they can withstand harsher conditions before reaching their breaking points.
NASA's 3D-printed superalloy can take the heat
by Brian Newbacher for GRC News
Washington DC (SPX) Apr 24, 2023

NASA has demonstrated a breakthrough in 3D printable high-temperature materials that could lead to stronger, more durable parts for airplanes and spacecraft.

A team of innovators from NASA and The Ohio State University detailed the characteristics of the new alloy, GRX-810, in a peer-reviewed paper published in the journal Nature.

"This superalloy has the potential to dramatically improve the strength and toughness of components and parts used in aviation and space exploration," said Dr. Tim Smith of NASA's Glenn Research Center in Cleveland, lead author of the Nature paper. Smith and his Glenn colleague Christopher Kantzos invented GRX-810.

Smith and his team employed time-saving computer modeling, as well as a laser 3D printing process that fused metals together, layer-by-layer, to create the new alloy. They used this process to produce the NASA logo pictured above.

GRX-810 is an oxide dispersion strengthened alloy. In other words, tiny particles containing oxygen atoms spread throughout the alloy enhance its strength. Such alloys are excellent candidates to build aerospace parts for high-temperature applications, like those inside aircraft and rocket engines, because they can withstand harsher conditions before reaching their breaking points.

Current state-of-the-art 3D printed superalloys can withstand temperatures up to 2,000 degrees Fahrenheit. Compared to those, GRX-810 is twice as strong, over 1,000 times more durable, and twice as resistant to oxidation.

"This new alloy is a major achievement," said Dale Hopkins, deputy project manager of NASA's Transformational Tools and Technologies project. "In the very near future, it may well be one of the most successful technology patents NASA Glenn has ever produced."

A team of contributors from Glenn, NASA's Ames Research Center in California's Silicon Valley, NASA's Marshall Space Flight Center in Huntsville, Alabama, and The Ohio State University co-authored the Nature paper.

GRX-810 was developed under NASA's Transformational Tools and Technologies project, with support from the agency's Game Changing Development Program.

Related Links
Aeronautics at NASA
Space Technology News - Applications and Research

Subscribe Free To Our Daily Newsletters
Tweet

RELATED CONTENT
The following news reports may link to other Space Media Network websites.
TECH SPACE
SwRI joins new NASA institute to qualify, certify additive manufacturing methods
San Antonio TX (SPX) Apr 19, 2023
Southwest Research Institute will contribute to a new NASA institute to improve understanding and enable rapid certification of metal parts created using advanced additive manufacturing (AM) techniques. The Institute for Model-based Qualification and Certification of Additive Manufacturing (IMQCAM) will work to improve computer models of additively manufactured metal parts and expand their utility in spaceflight applications. Additive manufacturing uses 3D printing or rapid prototyping to build an ... read more

TECH SPACE
Raytheon to provide Patriot air defense system to Switzerland

Aegis Combat System intercepts target during flight test

Ukraine forces complete Patriot training in US: Pentagon

PAC-3 flight test paves the way for new Patriot software release

TECH SPACE
AMRAAM variant, AIM-120D-3, completes critical milestone

Raytheon Technologies selected by US Navy for anti-ship strike weapon

Partnering and integration speeds delivery of a hypersonic missile

Russia says fired anti-ship missiles at mock target in Sea of Japan

TECH SPACE
Built to bounce back researchers design drones to cope with collisions

LIDS: A sure shot against drones

Drones navigate unseen environments with liquid neural networks

Iran army gets 200 new 'strategic' drones: state media

TECH SPACE
Hughes introduces Smart Network Edge Software for critical DoD communications

42-satellite constellation will provide resilient, secure comms for US troops globally

Building a Secure Resilient Satellite Infrastructure for Europe

Raytheon and SpiderOak collaborate to secure satcoms in crowded LEO

TECH SPACE
Developing agile, reliable sensing systems with microbes

US announces new $325 mn military aid package for Ukraine

Boeing signs joint weapons development deal with South Korea

Xi says China must strengthen training for 'actual combat'

TECH SPACE
Highest military spending in Europe since Cold War: study

Australia unveils biggest defence reform in decades

Seoul says military aid for Ukraine 'depends on Russia'

Polish PM blasts 'short-sighted' European opening to China after Macron visit

TECH SPACE
Czechs seek to boost security with new US defence deal

China says UK 'clinging to the past' with FM speech

Russian military aircraft intercepted over Baltic Sea: Germany

Macron, Biden agree to 'engage' China on Ukraine: French statement

TECH SPACE
Subscribe Free To Our Daily Newsletters




The content herein, unless otherwise known to be public domain, are Copyright 1995-2024 - Space Media Network. All websites are published in Australia and are solely subject to Australian law and governed by Fair Use principals for news reporting and research purposes. AFP, UPI and IANS news wire stories are copyright Agence France-Presse, United Press International and Indo-Asia News Service. ESA news reports are copyright European Space Agency. All NASA sourced material is public domain. Additional copyrights may apply in whole or part to other bona fide parties. All articles labeled "by Staff Writers" include reports supplied to Space Media Network by industry news wires, PR agencies, corporate press officers and the like. Such articles are individually curated and edited by Space Media Network staff on the basis of the report's information value to our industry and professional readership. Advertising does not imply endorsement, agreement or approval of any opinions, statements or information provided by Space Media Network on any Web page published or hosted by Space Media Network. General Data Protection Regulation (GDPR) Statement Our advertisers use various cookies and the like to deliver the best ad banner available at one time. All network advertising suppliers have GDPR policies (Legitimate Interest) that conform with EU regulations for data collection. By using our websites you consent to cookie based advertising. If you do not agree with this then you must stop using the websites from May 25, 2018. Privacy Statement. Additional information can be found here at About Us.